refinishing
Refinishing is the often overlooked and vitally important stage between metalwork and paint which requires patience, sanding and a very fine touch. We use Glasurit 90 line epoxy primer and high build primer to transform bare metal into a perfectly smooth surface that is ready for paint. We also seal every weld seam with 3M epoxy sealer to both waterproof the chassis and create a more fluid transition between panels.